Effect of ozonated water on dentin bond strength
Journal of Baghdad College of Dentistry
View Archive Info| Field | Value | |
| Title |
Effect of ozonated water on dentin bond strength
|
|
| Creator |
Ibraheem, Adel F.
HabeeB, Hasanain M. |
|
| Description |
Background: The aim of the study was to evaluate the influence of ozonated water application on dentin shear bond strength. Materials and Methods: Ten dentin samples per group were pretreated as follows: (I) untreated served as –ve control, (II) sterile distilled water for 10 seconds served as +ve control, (III) 5.25% sodium hypochlorite (Sultan-USA) for 10 seconds, (IV) 0.2% chlorhexidine (Corsodyle®, England) for 10 seconds, and (V) 4mg/L ozonated water (Ozonesolution-Enaly, USA) for 10 seconds. Samples were bonded with type II DBA (Unibond 2-Ventura, Spain) based on two clinical steps, etch, prime and bond combined and restored with a composite (Ventura-Similux, Spain) according to the manufacturer instruction. After storage in water at 37°C for 2 days and thermo-cycled for 500 cycles, shear bond strength was measured using Instron machine. Data were analyzed using ANOVA and Student t-test. Results: There was high significant increase in bond strength for ozonated water treated samples compared to controls at P |
|
| Publisher |
College of dentistry/ University of baghdad
|
|
| Date |
2017-01-31
|
|
| Type |
info:eu-repo/semantics/article
info:eu-repo/semantics/publishedVersion Peer-reviewed Article |
|
| Identifier |
http://jbcd.uobaghdad.edu.iq/index.php/jbcd/article/view/1710
|
|
| Source |
Journal of Baghdad College of Dentistry; Vol 20 No 2 (2008); 33-37
2311-5270 1680-0087 |
|
| Language |
en
|
|
| Rights |
Copyright (c) 2017 Journal of Baghdad College of Dentistry
|
|